輕型輸送帶用來輸送物料或產(chǎn)品、由經(jīng)緯不同的滌綸纖維交織成骨架材料和橡膠材料或PVC、PU、PE復(fù)合而成,在使用中應(yīng)注意:要安裝正確、確保接口與轉(zhuǎn)向適應(yīng)、接口處是正方向運(yùn)轉(zhuǎn)還是反方向運(yùn)轉(zhuǎn),視機(jī)械機(jī)構(gòu)的工作情況而定。表面有刮板或毛刷等工作內(nèi)容的,應(yīng)考慮表面順方向運(yùn)轉(zhuǎn),表面無工作內(nèi)容的則考慮反面順方向運(yùn)轉(zhuǎn)。
The light conveyor belt is used to transport materials or products. It is composed of polyester fibers with different longitude and weft interwoven into skeleton materials and rubber materials or PVC, PU and PE. In use, attention should be paid to correct installation, ensuring that the interface is suitable for steering, and whether the interface operates in the positive or negative direction depends on the working condition of the mechanical mechanism. If there is work content such as scraper or brush on the surface, it shall be considered to run in the direction of the surface, and if there is no work content on the surface, it shall be considered to run in the direction of the opposite side.
在正確安裝的基礎(chǔ)上防止跑偏。機(jī)架材料一般由鐵或鋁合金所組成,而輸送帶是由橡塑或PVC等纖維材料所組成。跑偏調(diào)整不當(dāng)會(huì)造成輸送帶的損壞。此項(xiàng)工作應(yīng)請有經(jīng)驗(yàn)的技師耐心調(diào)整。
Prevent deviation on the basis of correct installation. The frame material is generally composed of iron or aluminum alloy, while the conveyor belt is composed of fiber materials such as rubber, plastic or PVC. Improper deviation adjustment will cause damage to the conveyor belt. This work should be patiently adjusted by experienced technicians.
輕型輸送帶采用是進(jìn)口的滌綸纖維和進(jìn)口橡塑材料,雖然在纖維的織造中和產(chǎn)品的硫化、塑化過程中已采取了強(qiáng)制拉伸,但在制成品后有一個(gè)回縮過程,在使用過程中這個(gè)回縮過程還是會(huì)延伸,故在初次調(diào)整不宜過緊,在運(yùn)行3~5天或40小時(shí)左右,再調(diào)整到適用狀態(tài)良好,此時(shí)帶體的內(nèi)部應(yīng)力分布已達(dá)到均勻狀態(tài)。此時(shí)的輸送帶不會(huì)有延伸。

The light conveyor belt is made of imported polyester fiber and imported rubber and plastic materials. Although forced stretching has been adopted in the process of fiber weaving and product vulcanization and plasticization, there is a retraction process after the finished product, and this retraction process will still extend during use. Therefore, it should not be too tight in the initial adjustment. It runs for 3 ~ 5 days or about 40 hours, Then adjust it to a good applicable state. At this time, the internal stress distribution of the belt body has reached a uniform state. The conveyor belt will not extend at this time.
1.每班設(shè)備運(yùn)行前、檢查輸送帶運(yùn)行情況,及時(shí)調(diào)整相關(guān)設(shè)備。防止輸送帶跑偏使輸送帶邊緣磨損加劇而損壞上下覆蓋膠。造成鋼絲繩外露和脫落。每班的班前檢查要形成記錄備查。
1. Before the equipment operation of each shift, check the operation of conveyor belt and adjust relevant equipment in time. Prevent the deviation of the conveyor belt from aggravating the wear of the edge of the conveyor belt and damaging the upper and lower covering glue. The steel wire rope is exposed and falls off. The pre shift inspection of each shift shall be recorded for future reference.
2.每周一次傳動(dòng)滾筒表面的附著物,防止由于滾筒表面外形不規(guī)則造成接頭受力不均勻而產(chǎn)生鼓泡,鋼絲繩抽動(dòng),硫化接頭伸長等影響接頭強(qiáng)度的情況出現(xiàn)。輕型輸送帶表面污漬,可使用中性洗衣粉,也可使用酒精、松香水擦拭。嚴(yán)禁使用純苯類化學(xué)物品。完成、調(diào)試運(yùn)轉(zhuǎn)并做好記錄。
2. Remove the attachments on the surface of the transmission drum once a week to prevent bubbling, wire rope twitching, vulcanization joint elongation and other conditions affecting the joint strength due to uneven stress on the joint caused by the irregular shape of the drum surface. Light conveyor belt surface stains, you can use neutral detergent, you can also use alcohol, pine perfume to wipe. Pure benzene chemicals are strictly prohibited. Clean up, commissioning and operation and make records.
3.每月檢查一次輸送帶接頭、硫化接頭是輸送帶強(qiáng)度的薄弱部分,接頭開縫更初表現(xiàn)為膠開裂,水通過芯膠的縫隙浸入鋼絲繩,造成鋼絲繩銹蝕,斷絲,抽動(dòng)等。應(yīng)定期檢查接頭伸長變化量,表面異常變化等情況,做好預(yù)防性檢查工作,對出現(xiàn)缺陷的硫化接頭及時(shí)進(jìn)行修補(bǔ)。
3. Check the conveyor belt joint and vulcanization joint once a month, which are the weak parts of the conveyor belt strength. The opening of the joint is initially characterized by rubber cracking, and water is immersed into the steel wire rope through the gap of the core rubber, resulting in steel wire rope corrosion, wire breakage, twitching, etc. Regularly check the change of joint elongation and abnormal surface changes, do a good job in preventive inspection, and repair the defective vulcanized joint in time.
4.如果發(fā)生輸送帶邊膠,覆蓋膠脫落,局部露出鋼絲繩等缺陷,應(yīng)及時(shí)進(jìn)行冷粘或硫化熱補(bǔ)。根據(jù)輸送帶局部缺損狀況,選擇冷補(bǔ),熱硫化,填充鋼絲繩等不同的修補(bǔ)方式,保持輸送帶表面完好。
4. In case of defects such as edge glue of conveyor belt, falling off of covering glue and partial exposure of steel wire rope, cold bonding or vulcanization and hot repair shall be carried out in time. According to the local defects of the conveyor belt, different repair methods such as cold repair, hot vulcanization and filling steel wire rope are selected to keep the surface of the conveyor belt intact.